From: Fabrication and characterization of multiphase bituminous materials for cold region pavements
Materials | -6 °C | -12 °C | -18 °C |
---|---|---|---|
Mixture vs. FAM | 0.9618 | 0.9471 | 0.9208 |
Mixture vs. Masticmixture | 0.5785 | 0.6479 | 0.6814 |
Mixture vs. MasticFAM | 0.5481 | 0.5835 | 0.6231 |
Mixture vs. Binder | 0.5305 | 0.5462 | 0.5604 |
FAM vs. Masticmixture | 0.5850 | 0.6654 | 0.7275 |
FAM vs. MasticFAM | 0.5521 | 0.5934 | 0.6463 |
FAM vs. Binder | 0.5330 | 0.5517 | 0.5718 |
Masticmixture vs. MasticFAM | 0.8265 | 0.8023 | 0.8215 |
Masticmixture vs. Binder | 0.6940 | 0.6563 | 0.6578 |
MasticFAM vs. Binder | 0.8166 | 0.8068 | 0.8154 |