Table 1 Parameters entered in FEM

From: Chloride ion erosion of pre-stressed concrete bridges in cold regions

Parameter

Value

Parameter

Value

Cs0

0

nin

8.1

Csmax

0.37%

T

278.3 K

C

0.18738

q

5175.25

kc

1.4786

kT

0.3808

nact

93.38

kk

4.223

S

11.5

R

2.14

kw

1

D0

1.30 × 10–11 m2/s

w/c

0.45