Table 7 Assessment standard of pavement fatigue damage based on the miner criterion

From: Analysis methodology and assessment indices of vulnerability for asphalt pavement in cold regions

Assessment Index Micro Mild Moderate Severe Extreme
Cumulative damage degrees < 0.2 0.2 ~ 0.4 0.4 ~ 0.6 0.6 ~ 0.8 ≥0.8
The remaining service life (%) ≥0.8 0.6 ~ 0.8 0.4 ~ 0.6 0.2 ~ 0.4 < 0.2