Fig. 8

From: Petrographically quantifying the damage to field and lab-cast mortars subject to freeze-thaw cycles and deicer application

Fig. 8

a-b RLP and c-d BSE images of Ca-Oxy (blue solid dots) on a fracture surface of the damaged lab-cast paste in (a/c) an originally wet condition and (b/d) a dried condition, respectively. e EDX spectra obtained from zones in Figs. 7c and 8c-d. f Relationship between Ca and Cl contents of Ca-Oxy observed from EDX overlaid with theoretical Ca-Oxy formulae