Skip to main content

Table 1 Materials

From: Tensile mechanical properties of fly ash concrete at early age for thermal stress analysis

Property Materials Density
Water Tap water 1.00 g/cm3
Cement Ordinary Portland cement 3.16 g/cm3
Fly ash Class II 2.24 g/cm3
Fine aggregate Crashed sand 2.62 g/cm3
Coarse aggregate 1 Crashed stone 20–15 mm 2.67 g/cm3
Coarse aggregate 2 Crashed stone 15–5 mm 2.67 g/cm3
Admixture 1 Air entraining water reducing agent 1.07 g/cm3
Admixture 2a Air entraining agent for fly ash 1.04 g/cm3
  1. a: diluted solution (diluted 100 times with water)